Share on:
See more product details Thermal Shock Resistance - average coefficient of expansion from 20° C to 200° C is 3.56 x 10-5, gradually increasing to 4.69 x 10-5 at 1050°C. Every batch of porcelain is heat tested in our factory. Glaze - No softening occurs up to 1000°C, and it is extremely white. Resistance to Chemical Action - Resistance to acids and alkalies is excellent, except for hydrofluoric acid. To calculate the overall star rating and percentage breakdown by star, we don’t use a simple average. Instead, our system considers things like how recent a review is and if the reviewer bought the item on Amazon. It also analyzed reviews to verify trustworthiness.